Plenary 3- The failure of adhesive layers: from fast fracture to stress corrosion

Plenary 3- The failure of adhesive layers: from fast fracture to stress corrosion

Norman Fleck

Adhesive joints are increasing used in engineering components, particularly in the bonding of dissimilar materials. This talk focuses on deformation and failure mechanisms of a sandwich joint: brittle fracture in elastic layers, ductile failure by cohesive zone modelling, diffusion-controlled attack of an interface and toughening of an adhesive layer by the presence of micro-architectured reinforcement.